XRD measurement settings.

Sample Angle Range (2Theta) Incident Beam Diffracted Beam Detector
Powdered Mg2Sn alloy 20–90° Divergence slit: 1/2°
Soller slit: 0.04 rad
Anti-scatter slit: 1°
Anti-scatter slit: 1°
Soller slit: 0.04 rad
PIXcel3D detector in 1D scanning mode
Powdered corrosion products 20–90° Divergence slit: 1/4°
Soller slit: 0.04 rad
Anti-scatter slit: 1/2°
Anti-scatter slit: 1/2°
Soller slit: 0.04 rad
PIXcel3D detector in 1D scanning mode