Skip to main content
. 2022 Mar 21;15(6):2335. doi: 10.3390/ma15062335

Table 4.

Dependence of the efficiency of immobilization of Cr (VI) as a percentage of the SCS type and the amount of Carbofill E.

Type of SCS SCS Samples Carbofill E, %
10 15 20
sandy undisturbed 99.9980 99.9978 99.9988
crushed 99.4 99.633 99.980
clay undisturbed 99.9970 99.9983 99.99197
crushed 97.847 99.655 99.806

3000 mg/kg Cr (VI) was added to the SCS samples.