Table 3. Experimental Scheme of Single Proppant Conductivity.
| experiment no. | proppant type | proppant size (mesh) | bulk density (g/cm3) | pack thickness (mm) | proppant concentration (kg/m2) | proppant mass (g) |
|---|---|---|---|---|---|---|
| 1 | ceramic | 20/40 | 1.46 | 5 | 7.3 | 47.09 |
| 2 | 40/70 | 1.43 | 5 | 7.2 | 46.12 | |
| 3 | sand | 20/40 | 1.53 | 5 | 7.7 | 49.34 |
| 4 | 40/70 | 1.47 | 5 | 7.4 | 47.14 |