Cone calorimetry results of POSS/D-bp/DGEBA hybrid compositesa,b,c,d.
| Samples | TTI (s) | P-HRR (kW m−2) | THR (MJ m−2) | av-EHC (MJ kg−1) | P-SPR (m2 s−1) | Residues (wt%) |
|---|---|---|---|---|---|---|
| EP-1 | 53 | 939 | 202 | 31.6 | 0.35 | 13.5 |
| EP-2 | 48 | 753 | 175 | 29.2 | 0.33 | 17.1 |
| EP-3 | 53 | 767 | 134 | 29.0 | 0.30 | 17.3 |
| EP-4 | 54 | 371 | 116 | 23.9 | 0.22 | 25.9 |
| EP-5 | 49 | 651 | 130 | 23.6 | 0.29 | 18.1 |
| EP-6 | 51 | 361 | 115 | 21.3 | 0.20 | 28.5 |
P-HRR: under the preset incident heat flux intensity, the maximum value of heat release rate per unit area after the material is ignited.
THR: the sum of the heat released by the material from ignition to flame extinction under the preset incident heat flow intensity.
EHC: the ratio of measured heat release rate to mass loss rate at a certain time reflects the combustion degree of volatile gas in gas phase flame.
P-SPR: the maximum value of specific extinction area (SEA) to mass loss rate (MLR).