The electrochemical parameters extracted from the fitting of the EIS results of the neat epoxy sample after immersion in a corrosive 3.5% NaCl solution at various immersion times.

Sample Time [day] R s [Ω cm2] Q coat [10−9 F cm2 sn−1] n 1 R coat [104 Ω cm2] Q dl [10−7 F cm2 sn−1] n 2 R ct [105 Ω cm2]
Epoxy 3 3.2 2.91 1.00 61.24
6 4.9 2.59 0.95 49.31 5.49 0.97 34.12
10 2.3 1.98 0.92 45.54 9.26 0.94 29.81
14 1.8 2.65 0.88 29.18 10.9 0.93 9.21
18 1.3 5.29 0.87 5.31 14.71 0.87 7.51
21 1.3 27.18 0.76 2.70 69.16 0.79 4.22