Figure 12.

Figure 12

(a) Current–potential curves of NiO/PRu-PolyPyr-Ru-RuCAT under irradiation at λex = 460–650 nm (28.2 mW cm–2) in CO2-purged 50 mM aqueous NaHCO3. (b) Dependence of the IPCE of NiO/PRu-PolyPyr-Ru-RuCAT by the irradiated wavelength at −0.3 V vs Ag/AgCl with absorption spectrum of NiO/PRu-PolyPyr-Ru-RuCAT subtracted with the absorbance of the NiO electrode (red line).