Figure 2

AFM surface images (3D-left) and SEM micrographs (right) on p(NIPAM-BA) coatings when DMSO was used as solvent; (A,E) drop-cast and MAPLE deposition on Si at 250 mJ/cm2 (B,F), 350 mJ/cm2 (C,G), and 450 mJ/cm2 fluences (D,H). The AFM images correspond to areas of 5 × 5 µm2 and 2 × 2 µm2; SEM magnifications 40,000×.