. 2022 Mar 31;15(7):2556. doi: 10.3390/ma15072556

Table 1.

Thermal decomposition temperatures of EPDM, silica and EPDM-based MRE samples.

Sample Tonset (°C) T50% (°C) Tp (°C) Residue (%)
EPDM 426.3 454.6 464.3 0.891
S1 (0 wt.% SiO2) 430.3 463.9 468.5 41.09
S2 (3 wt.% SiO2) 434.9 464.8 469.8 48.06
S3 (6 wt.% SiO2) 435.8 465.1 471.1 48.3
S4 (9 wt.% SiO2) 437.7 467.4 472.7 49.17
S5 (11 wt.% SiO2) 438.5 469.5 473.5 50.68