Skip to main content
. 2022 Mar 24;12(7):1068. doi: 10.3390/nano12071068

Table 4.

The Raman spectra behavioral differences between the clear PC and the TiC samples.

Wavenumber (cm−1) Assignment Change
631 Phenyl ring vibration Increased vibration for TiC samples
647 Phenyl ring vibration New peak for TiC samples
700 C-H out-of-plane bending Increase of peak for TiC samples
883 ν[O-(C=O)-O], ν(C-CH3), r(CH3), ν(ring) Increase of peak for TiC samples
1106 C-O-C stretching Increase of peak for TiC samples
1175 C-O-C stretching Increase of peak for TiC samples
1231 C-O-C group asymmetric vibration Increase of peak for TiC samples
1740 C=O vibration New peak for TiC samples
2912 CH2vAS or C-H Gradual increase vs. TiC concentration
2911 CH2vAS or C-H Constant
2970 CH/CH2 stretch modes polarized Constant
3071 C-H stretching Gradual increase vs. TiC concentration