Data obtained from citrate-coated AuNPs dispersions and from the biosensors (pAb-AuNPs).

Size DHa AuNP/nm PDIb λmaxc/nm [AuNP]/NP /mL [AuNP]/μg/mL Sd/nm2/NP Sd/nm2/mL DHa DTSSP-AuNP/nm DHa pAb-AuNP/nm (35 μg/mL)
S44 49 ± 12 0.22 525 21 × 1010 175 6 × 103 13 × 1014 50 ± 12 70 ± 18
S64 65 ± 15 0.21 536 8.4 × 1010 222 13 × 103 11 × 1014 61 ± 17 85 ± 20
S87 74 ± 18 0.25 552 3.6 × 1010 241 24 × 103 8.6 × 1014 91 ± 22 117 ± 28
S101 88 ± 22 0.26 556 2.4 × 1010 246 32 × 103 7.7 × 1014 95 ± 25 109 ± 26
S130 121 ± 27 0.19 583 1.1 × 1010 251 53 × 103 5.8 × 1014 128 ± 30 146 ± 30
a

Hydrodynamic diameters.

b

Polydispersity index (PDI) of citrate-coated AuNPs.

c

Plasmonic resonance peak.

d

Surface area of AuNPs.