Survival of metal-ceramic and all-ceramic fixed partial dentures.

Study Year Total No. of FPDs Mean Follow-Up Time No. of Failures Estimated Annual Failures Estimated Survival in % after
(N) = Years
Metal-ceramic
Chirstensen et al. [37] 2010 69 n.r. 0 1.6 (3) 95%
Nicolaisen et al. [45] 2016 17 n.r. 0 0 (3) 100%
Sailer et al. [46] 2018 24 10.0 1 0 (10) 100%
Suarez et al. [47] 2019 20 5.25 ± 0.2 0 0 (5) 100%
Forrer et al. [50] 2020 30 6.44 ± 1.14 1 0.72 (5) 96.4%
Reinforced glass-ceramic
Makarouna et al. [38] 2011 18 4.7 6 7.14 (5) 70%
Kem et al. [39] 2012 36 10.1 4 1.10 (5) 94.6%
Sola-Ruiz et al. [40] 2013 21 10.0 6 2.86 (5) 86.7%
Brandt et al. [49] 2019 136 3.10 ± 1.5 8 0.93 (5) 9.35%
Glass-infiltrated alumina
Christensen et al. [37] 2010 34 n.r. 11 10.6 (3) 68%
Zirconia
Christensen et al. [37] 2010 163 n.r. 2 4.66 (3) 86%
Koenig et al. [41] 2013 30 3.96 ± 2.7 1 2.04 (9) 81.6%
Rinke at al. [42] 2013 99 6.3 19 3.03 (5) 85.9%
Haff et al. [43] 2015 33 9.6 ± 1.6 2 0.6 (10) 94%
Ioannidis et al. [44] 2016 57 6.3 ± 1.9 3 1.5 (10) 85%
Nicolaisen et al. [45] 2016 17 n.r. 0 0 (3) 100%
Sailer et al. [46] 2018 29 10.3 5 0.87 (10) 91.3%
Saurez et al. [47] 2019 20 5.25 ± 0.2 0 0 (5) 100%
Koenig et al. [48] 2019 10 n.r. 1 0 (3) 100%
Forrer et al. [50] 2020 53 6.44 ± 1.14 2 0.42 (5) 97.9%