. 2022 Apr 12;15(8):2813. doi: 10.3390/ma15082813

Figure 6.

Figure 6

Microscopic corrosion morphology under SEM after immersion in 3.5% NaCl solution saturated with Mg(OH)2 for 24 h: (a,b) As-extruded sample; (c,d) T5 sample; (e,f) T6 sample.