Skip to main content
. 2022 Apr 14;14(8):1603. doi: 10.3390/polym14081603

Figure 3.

Figure 3

PLA beads coated with GS-doped mHNTs in Mueller–Hinton broth for 48 h with S. aureus. Optical density readings were taken at 0, 24, and 48 h. Optical density was taken at 630 nm wavelength. Error bars represent ± standard deviation (n = 3).