Figure 1. Impact of water vapor annealing time on DNX release.

Figure 1.

Cumulative release of DNX-loaded silk foams was evaluated. DNX-loaded silk foams were exposed to water vapor for 4 h, 8 h, and 24 h. Data are presented as mean ± standard deviation of three independent samples.