Skip to main content
. 2022 Apr 27;12:6834. doi: 10.1038/s41598-022-10879-5

Table 1.

Comparison of the performances of core–shell nanowire arrays based photodetectors.

Nanowires materials Bias Range of detection Responsivity Detectivity Rise time/decay time References
CuO–ZnO core–shell 0.5 V VIS 26.3 A/W 5.8 × 1013 Jones 0.5 s/0.5 s This work
ZnO/Cu2O core–shell 5 V UV 26.9 A/W 6.3 × 109 Jones 1.4 s/3.4 s 55
ZnO/Cu2O core–shell 0 V VIS 7.6 µA/W 0.09 s/0.09 s 56
ZnO/Co3O4 core–shell 0.1 V VIS 21.8 mA/W 4.1 × 1012 Jones 6 s/– 35
ZnO/Ga2O3 core–shell 0 V UV 137.9 mA/W 6.1 × 1012 Jones 28.9 µs/85.7 µs 53
ZnO/ZnS core–shell 1.5 V UV 0.2 A/W 57
ZnO/CuCrO2 core–shell − 1 V UV 5.87 mA/W 8.5 × 109 Jones 32 µs/35 µs 33