Skip to main content
. 2020 Jan 27;10(8):4218–4231. doi: 10.1039/c9ra10857b

Fig. 2. Effect of varying formulation parameters on nanoparticle diameter size. (A) PLGA concentration; (B) PVA concentration; (C) organic solvent fraction; and (D) speed of agitation in evaporation. Preparations by the emulsification technique with PLGA of 17 kg mol−1, P17A-E (Inline graphic). Preparations by the nanoprecipitation technique with PLGA of 17 kg mol−1, P17A-N (Inline graphic), and PLGA of 153 kg mol−1, P153-N (Inline graphic). Data represent mean ± SD (n = 3).