. 2020 Jan 28;10(8):4650–4656. doi: 10.1039/c9ra09714g

Fig. 5. (a) Cyclic voltammograms at different sweep rates, (b) galvanostatic charge–discharge profiles at various applied current densities, (c) corresponding Ragone plot, and (d) plot of the cyclic stability for the NiCoP-modified electrode in 5 M KOH electrolyte.