Skip to main content
. 2020 Feb 13;10(12):6840–6849. doi: 10.1039/c9ra10464j

Fig. 3. (a) Typical DTA/TG/DTG curves of the decomposition of Ti(OBu)4/polymer precursor nanofibers with ×1.0 TiO2/polymer yield mass ratio and 1 : 1 PVP/HPC mass ratio; (b) mass loss of precursor fibers with different TiO2/polymer yield mass ratios during calcination after initial stabilization at 120 °C.