. 2020 Feb 13;10(12):6840–6849. doi: 10.1039/c9ra10464j

Fig. 6. XRD patterns of TiO2 nanofibers prepared from the precursors with different TiO2/polymer yield mass ratios after calcination at (a) 500 °C and (b) 750 °C. Symbols ● – indicate the peaks from anatase and ♦ – from rutile; (c) rutile content and (d) anatase and rutile crystallite size in TiO2 nanofibers after calcination at 500 °C and 750 °C vs. the precursor composition. Dotted lines show general trend.