. 2020 Feb 13;10(12):6777–6789. doi: 10.1039/c9ra10414c

Fig. 1. SZP results from EOF measurements for RO membrane using latex tracer particles as a function of the ionic strength (a). Exemplarity apparent zeta potential at different displacement in 2 mM KCl (b) and corresponding phase plots (c). Size distribution of the latex tracer particles after EOF measurement at 5 mM ionic strength (d).

Fig. 1