Thickness, porosity, tensile strength and elongation at break of the papers before and after surface coating.

Sample Thickness (μm) Porosity (%) Tensile strength (MPa) Elongation at break (%)
Paper 265.4 ± 3.4 87.4 ± 1.3 7.8 ± 0.6 23.8 ± 2.3
PDA/paper 287.4 ± 3.6 81.2 ± 1.7 8.4 ± 0.5 26.3 ± 1.0
PDMS–SiO2/PDA/paper 298.8 ± 5.1 77.0 ± 2.1 7.7 ± 0.8 27.5 ± 1.6
PDMS–SiO2/paper 293.4 ± 7.4 69.2 ± 3.5 8.1 ± 0.7 28.9 ± 2.7