. 2020 Mar 10;10(17):10155–10166. doi: 10.1039/c9ra10874b

Fig. 5. Growth of healthy HaCaT cells on POEGMA188-based nanocomposite coatings fabricated for 16 hours of polymerization (a, c and e) and POEGMA188 with incorporated AgNPs obtained after 15 min of immersion at 5 mM AgNO3 solution followed by reduction in 0.2 M NaBH4 solution for 12 h (b, d and f).

Fig. 5