Skip to main content
. 2020 Mar 20;10(19):11426–11434. doi: 10.1039/c9ra10702a

Fig. 6. FESEM microstructures of the epoxy and octylamine-functionalized GO-coated Mg alloys after immersion in the 3.5% NaCl environment for 5 days (A) epoxy coated Mg alloy, (B) uniform oxide layer formed on surface, (C and D) alkyl amine functionalized GO coated magnesium alloy surface.

Fig. 6