Oxidation state of platinum (δ) and Pt L3-edge EXAFS fitting results (R, distance; CN, coordination number; σ2 Debye–Waller factor; ΔE0, inner potential correction b) of Pt–Nb2O5 samples.

Sample δ Pt–O Pt–Pt σ 22) ΔE0 (eV)
R (Å) CN R (Å) CN
1 Pt–Nb2O5-fresh 1.82 ± 0.04 1.98 ± 0.01 4.1 ± 0.2 0.003(O)0.005 ± 0.001(Pt) 12.1 ± 0.7
1 Pt–Nb2O5–H2 1.20 ± 0.02 2.00 ± 0.01 2.2 ± 0.2 10.2 ± 2.5
1 Pt–Nb2O5-used 1.01 ± 0.02 1.97 ± 0.01 1.9 ± 0.2 2.70 ± 0.02 1.8 ± 0.6 8.3 ± 1.4
0.3 Pt–Nb2O5-fresh 1.84 ± 0.02 1.98 ± 0.01 4.1 ± 0.3 12.1 ± 0.7
0.3 Pt–Nb2O5–H2 1.13 ± 0.02 2.00 ± 0.02 2.3 ± 0.5 10.2 ± 2.5
0.3 Pt–Nb2O5-used 0.72 ± 0.02 1.97 ± 0.01 1.7 ± 0.3 2.74 ± 0.01 4.9 ± 1.2 8.3 ± 1.4