Skip to main content
. 2020 Mar 23;10(20):11777–11790. doi: 10.1039/d0ra00517g

Mooney–Rivilin and tube model parameters for XNBR75/CR25 nanocomposites containing the XNBR-g-GMA compatibilizer and different amounts of graphene (0.1, 0.3, 0.5, 0.7 and 1).

Blends C 1 C 2 graphic file with name d0ra00517g-t14.jpg G C V C × 104 (mol cm−3) M C (g mol−1) R C (nm) N G e (MPa) d 0 (nm) n e
75/25/0 (W C) 0.0701 0.9711 0.2281 0.8001 2.621 2832 3.885 23 0.8312 1.821 4.8577
75/25/0 0.0899 0.9698 0.2355 0.8108 2.911 2911 4.112 24 0.8896 1.774 4.6352
75/25/0.1 0.1655 0.8662 0.2448 0.8309 3.069 2976 4.239 24 1.1254 1.656 4.3211
75/25/0.3 0.2889 0.7359 0.2722 0.8558 3.448 2989 4.339 24 1.1879 1.5521 4.0012
75/25/0.5 0.3621 0.7301 0.2801 0.8752 4.006 3099 4.774 25 1.2254 1.4412 3.8321
75/25/0.7 0.3889 0.6758 0.2902 0.8821 4.125 3112 4.811 25 1.2879 1.3987 3.3589
75/25/1 0.4001 0.6235 0.2895 0.8806 4.133 3158 4.889 25 1.2888 1.3882 3.0123