. 2020 Mar 23;10(20):11777–11790. doi: 10.1039/d0ra00517g

DMTA data of XNBR75/CR25 nanocomposites (effect of graphene and compatibilizer).

Samples T g from E′ [°C] T g from tan δ [°C] T i from tan δ [°C] Height of Tg peak [—] Decrease in tan δ peak [—] Height of Ti peak [—] E′ at 25 °C [MPa]
75/25 (W C) −3.52 −1.89 — 5.92 0 — 3.02
−27.92 −25.59 — 2.44 0 — 6.71
75/25/0 −2.33 −1.06 — 2.98 2.94 — 8.55
75/25/0.1 −1.31 1.57 51.21 2.34 3.58 0.311 9.33
75/25/0.3 0.22 2.45 50.28 2.01 3.91 0.329 9.91
75/25/0.5 1.93 3.01 49.33 1.81 4.11 0.388 10.55
75/25/0.7 2.41 4.08 47.55 1.61 4.31 0.418 10.98
75/25/1 3.13 5.55 46.39 1.52 4.39 0.438 11.33