Skip to main content
. 2022 Apr 28;13:2320. doi: 10.1038/s41467-022-29970-6

Fig. 3. Characterization and activity of the AlOOH catalyst.

Fig. 3

a XRD b FTIR c O1s and d Al 2p XPS and e Reactivity comparison of different catalyst. f Catalyst recycling of AlOOH-U2. Catalyst (50 mg), temperature (80 °C), H2 pressure (2 MPa), time (6 h), styrene (0.5 mmol), THF (2 mL), stirring speed (600 rpm) and n-decane as internal standard.