Skip to main content
. 2020 Apr 1;10(22):13316–13368. doi: 10.1039/d0ra01801e

Fig. 37. SEM images of PLA/PBAT (90/10) (a and a′) and PLA/PBAT/EMA-GMA (82/10/8) (b and b′) and PLA/PBAT/EMA-GMA (75/10/15) (c and c′) blends at impact fracture and cryofracture surfaces. Ref. 166, copyright 2017. Reproduced with permission from Elsevier.

Fig. 37