XRD parameters of An before and after impregnation with CNTs by calcination at 950 °C/2 h.

Sample 2θ002 (°) d spacing (height between adjacent layers in the c direction), dc (Å) Crystallite stacking height Lc (Å) Crystallite size La (Å) Staking layer number n (Lc/d002)
An 26.63 3.348 270.59 404.76 80.82