Coercivity Fields, Hc, and saturation magnetization, Ms, of ε-Fe2O3 and γ-Fe2O3 NPs suspensions, before and after polymer coating, at different temperatures.

Phase Coating H c (Oe) Ms (emu per g Fe2O3)
200 K 250 K 300 K 200 K 250 K 300 K
ε-Fe2O3 No 20 500 1900 0 9 10 10
Yes 20 000 3300 0 10 15 15
γ-Fe2O3 No 33 23 0 76 74 74
Yes 36 19 0 72 69 72