Skip to main content
. 2020 Oct 8;10(61):37314–37326. doi: 10.1039/d0ra07521c

Thermal degradation properties of PBS nanocomposites.

3CTA-BDT in PBS T d (5%) T d (10%) T d (50%) T d (dTGA) (°C) Residue at 550 °C (%)
0% (pure PBS) 320 353 392 396 2.31
1% 354 368 400 400 3.16
3% 349 363 395 399 2.84
5% 312 347 395 400 2.77