Skip to main content
. 2019 Apr 12;9(21):11602–11613. doi: 10.1039/c9ra00645a

Rheological aging index (RAI) for binder B502.

Asphalt binder Area under the master curve Area between virgin and aged binder (rheological aging index – RAI) % of virgin area
B502 1.67 × 107
B502B_123 1.90 × 107 2.28 × 106 13.7
B502B_163 2.35 × 107 6.86 × 106 41.2
B502C_123 3.73 × 107 20.63 × 106 124.0
B502C_163 4.05 × 107 23.82 × 106 143.0