Magnetic parameters calculated from the VSM data of K2 and K3 beads at 5 and 300 K.

Material Temperature (K) Saturation magnetization (Ms) (emu g−1) Coercivity (Hs) (tesla) Permanent magnetization (Mr) (emu g−1)
K2 beads 5 3.391 0.02377 0.46839
300 3.158 0.00435 0.03588
K3 beads 5 4.315 0.02761 0.80530
300 3.602 0.00370 0.06078