. 2022 Mar 8;9(13):2104788. doi: 10.1002/advs.202104788

Figure 2.

Figure 2

a) Variation of the thickness of the MAPbBr3 SCTFs with the dead load on the sandwiched structures, b) TRPL decay transients of the MAPbBr3 SCTFs under 405 nm excitation, c) XRD patterns for MAPbBr3 SCTFs prepared under various heating rate at room temperature (25 °C), and d–f) high‐resolution XRD rocking curves of the (200) diffraction peaks of the MAPbBr3 SCTFs at a heating rate of d) 10 °C h−1, e) 5 °C h−1, and f) 2 °C h−1.