Raw materials used for synthesis of dialdehyde lignocellulose and results of their characterizationa.
Name | Kappa number | Cellulose content (wt%) | Xylan content (wt%) | Total lignin content (wt%) |
---|---|---|---|---|
Commercially available Eucalyptus bleached kraft pulp b | ||||
Cp | — | 85 | 14 | <0.1 |
Eucalyptus wood wastes pulps c | ||||
D2 | 10.2 | 90.2 | 7.3 | 1.9 |
D3 | 13.9 | 89.6 | 7.2 | 2.8 |
D1 | 16.1 | 76.7 | 17.5 | 2.2 |
D4 | 26.7 | 71.6 | 18.3 | 4.4 |
Cp: commercially available bleached pulp; D2 and D3: pulps obtained by kraft cooking with previous hot water extraction of the wood wastes; D1 and D4: pulps obtained by kraft cooking.
Values taken from the literature.22
Xylan content does not include substituent acid groups.