Comparison of electrode properties with reported literature.
| Sample | Specific capacitance | Working potential | Electrolyte | Energy density, power density | Supp. ref. |
|---|---|---|---|---|---|
| NiO@MnO2 core–shell structure | 766.8 F g−1 (10 A g−1) | 0–0.5 V vs. SCE | 2.0 M KOH | — | 35 |
| NiO@MnO2 core–shell nanocomposite | 266.7 F g−1 (0.5 A g−1) | 0–0.45 V vs. SCE | 2.0 M KOH | — | 36 |
| NiO/MnO2 core–shell nanoflakes | 241 mF cm−2 (1 mA cm−2) | 0–0.7 V vs. SCE | 1.0 M KOH | — | 37 |
| NiO/MnO2 core–shell composite | 528 F g−1 (1 mV s−1) | 0–0.5 V vs. Ag/AgCl | 1 M LiOH | — | 30 |
| NiO/MnO2 core–shell composite | 558 F g−1 (5 mA cm−2) | 0–0.5 V vs. SCE | 6.0 M KOH | 20.37 W h kg−1, 133.3 W kg−1 | This work |