Skip to main content
. 2018 Jan 15;8(6):3120–3131. doi: 10.1039/c7ra12309d

Fig. 4. XRD patterns (λ = 0.4959 Å) of the initial rhombohedral LSF sample (black) and cubic LSF after cool-down to room temperature following the treatment in hydrogen to 873 K (red). The insets show the characteristic differences between the two different structures.

Fig. 4