Skip to main content
. 2018 Mar 13;8(18):10124–10140. doi: 10.1039/c8ra00069g

Fig. 11. (a) Concentration changes (C/C0) and (b) plot of −ln(C/C0) versus irradiation time of MB dye over APO/C60(5), m-APO/C60(10), m-APO/C60(20) and pure APO photocatalysts. Experimental conditions: [MB] = 25 mg L−1, [catalyst] = 0.05 g and [H2O2] = 30 wt%, 0.5 mL under visible light irradiation for 5 h.

Fig. 11