Magnetic properties of the pure Fe3O4 sample and the m-APO/C60 nanocomposites.

Sample Magnetic remnant (Mr) (emu g−1) Magnetic saturation (Ms) (emu g−1) Coercivity field (Hc) (Oe)
Fe3O4 3.68 57.84 31.46
m-APO/C60(5) 0.76 21.15 30.28
m-APO/C60(10) 3.13 18.55 60.69
m-APO/C60(20) 0.58 10.59 50