The characteristics of hydrogels with different PPy mass ratio.
Sample | Swelling ratio (w/w) | Porosity (%) | Conductivity (S cm−1) |
---|---|---|---|
SA/CMCS/PPy(0.02) | 9.132 | 86.69 | 7.35 × 10−6 |
SA/CMCS/PPy(0.05) | 9.020 | 84.27 | 2.41 × 10−5 |
SA/CMCS/PPy(0.10) | 8.461 | 80.54 | 4.71 × 10−5 |
SA/CMCS/PPy(0.20) | 7.511 | 73.16 | 1.42 × 10−3 |
SA/CMCS/PPy(0.40) | 5.013 | 62.87 | 8.03 × 10−3 |