Skip to main content
. 2018 Apr 9;8(24):13075–13082. doi: 10.1039/c8ra00463c

Results from Ag35Al65 samples dealloyed with water in supercritical CO2 (termed W-SC) at 120 °C and 2000 psi, for 30 and 60 min.

Pre-dealloyed Dealloyed using W-SC at 120 °C and 2000 psi for 30 min Dealloyed using W-SC at 120 °C and 2000 psi for 60 min
EDS results Ag35Al65 Ag53Al47 Ag59Al41
Surface area (m2 g−1) 0 1.9 2.5
Porosity 0% 25% 32%
Average pore size (nm) ∼200 ∼200