Skip to main content
. 2018 Apr 6;8(23):12933–12943. doi: 10.1039/c8ra01305e

Structural parameters of sc-PLA/PBAT scaffolds prepared with different water/dichloromethane ratios.

Samples 0.4/1 0.5/1 0.6/1 0.7/1 0.8/1 0.9/1
Porosity (%) 34.6 61.2 88.0 92.6 94.1 93.5
Surface area (m2 g−1) 2.04 3.17 7.22 9.43 10.61 9.21
Average diameter (μm) 0.76 1.58 1.04 1.76 3.96 4.52