Skip to main content
. 2018 May 4;8(30):16619–16625. doi: 10.1039/c8ra01565a

The experimental parameters used for the electrospinning preparation of various nanofiber membranesa.

Sample Core Sheath Voltage Injecting Speed
P 8% PLA +8.5 kV to 2.5 kV 0.86 mL h−1
S15 8% PLA + 15 mg mL−1 GO +8.5 kV to 2.5 kV 0.86 mL h−1
C5 5 mg mL−1 GO 8% PLA +8.5 kV to 2.5 kV 0.06 mL h−1 @ 0.8 mL h−1
C15 15 mg mL−1 GO 8% PLA +8.5 kV to 2.5 kV 0.06 mL h−1 @ 0.8 mL h−1
C25 25 mg mL−1 GO 8% PLA +8.5 kV to 2.5 kV 0.06 mL h−1 @ 0.8 mL h−1
a

P = pure PLA; S15 = single-axial structure with 15 mg mL−1 of GO; C5 = co-axial structure with 5 mg mL−1 of GO; C15 = co-axial structure with 15 mg mL−1 of GO; C25 = co-axial structure with 25 mg mL−1 of GO.