Skip to main content
. 2018 May 18;8(33):18334–18340. doi: 10.1039/c8ra02058b

Thermoelectric properties of PEDOT:PSS film with and without TFMS–MeOH treatment.

Sample S (μV K−1) δ (S cm−1) PF (μW m−1 K−2) C p (J K g−1) α (mm2 S−1) κ (W K−1 m−1)
Pristine 17.6 ± 1.5 0.7 ± 0.1 0.0216 ± 0.003 2.36 ± 0.05 0.074 ± 0.005 0.279 ± 0.030
TFMS–MeOH 21.9 ± 2.0 2980 ± 150 143 ± 15 1.87 ± 0.05 0.075 ± 0.005 0.224 ± 0.020