. 2018 Jun 8;8(38):21133–21138. doi: 10.1039/c8ra01256c

Fig. 4. Stress–strain curves for PDMS membrane. All data were obtained using the measurement devices (N = 3) with known dimensions (h = 0.25 mm, w = 1 mm, r = 2 mm). The PDMS membranes used for this experiment have a thickness of 35 μm.

Fig. 4