Skip to main content
. 2018 Jun 27;8(41):23274–23283. doi: 10.1039/c8ra03367f

Data obtained from the sorption/desorption isotherms for pectin–CaCO3 and NPEC–CaCO3 composite microparticles.

Pectin type an +/n bSC, % d.b. cAPS, nm dBET eGAB fDC
Area, m2 g−1 gM, g g−1 Area, m2 g−1 gM, g g−1 D 1, 10−8 cm2 s−1 D 2, 10−7 cm2 s−1
PCT49 0 1.57 2.97 10.60 0.003 13.70 0.0039 5.89 5.33
0.5 3.32 4.16 16.02 0.004 13.34 0.0038 5.41 6.98
0.9 4.66 3.28 28.50 0.008 17.85 0.0050 4.79 6.41
1.2 4.81 3.95 24.43 0.007 28.60 0.0081 4.90 7.09
PCT53_A21 0 1.63 2.40 13.62 0.004 13.77 0.0039 7.28 5.15
0.5 2.67 2.72 19.69 0.006 13.20 0.0037 5.76 6.53
0.9 4.13 3.81 21.73 0.006 23.81 0.0067 5.18 9.04
1.2 6.64 4.02 33.12 0.009 25.05 0.0071 4.04 5.45
a

NPEC molar ratio.

b

Sorption capacity.

c

Average pore size.

d

Brunauer–Emmett–Teller method.

e

Guggenheim–Anderson–de Boer method.

f

Diffusion coefficients.

g

Monolayer.