Skip to main content
. 2018 Sep 10;8(55):31529–31537. doi: 10.1039/c8ra06581k

Intensity of the diffraction peaks of CdS and PtNi3/CdS.

2θ Lattice plane I I PtNi3/CdS/ICdS
CdS PtNi3/CdS
25.09 (100) 2034 2119 1.042
26.77 (002) 19 096 5872 0.307
28.46 (101) 2416 2107 0.872
36.88 (102) 607 400 0.659
43.97 (110) 1984 2711 1.366
48.12 (103) 1851 1261 0.681
52.09 (112) 1578 2075 1.315