Information on the WC–Co samples used in the present study.

Sample Carbide grain size (μm) Cobalt fraction (wt%) Densification method11 Plastic deformation Group
1 1.0 6 Sinter-HIP No A
2 1.0 8 Sinter-HIP No A B C D
3 1.0 10 Sinter-HIP No A
4 2.0 8 Sinter-HIP No B
5 0.5 8 SPS No C
6 1.0 8 Sinter-HIP Yes D