Physicochemical data for the series of CHMS and LHMS samplesa.
| Sample | S BET (m2 g−1) | V P (cm3 g−1) | d-spacing (nm) | a (nm) | D KJS (nm) | W (nm) |
|---|---|---|---|---|---|---|
| CHMS-1 | 90.90 | 0.35 | 3.86 | 4.46 | 11.10 | n.d. |
| CHMS-2 | 317.73 | 0.40 | 3.90 | 4.50 | 3.23 | 1.27 |
| CHMS-3 | 35.63 | 0.18 | 3.90 | 4.50 | 15.37 | n.d. |
| CHMS-5 | 315.86 | 0.46 | 3.93 | 4.54 | 3.42 | 1.12 |
| LHMS-1 | 742.97 | 0.59 | 3.83 | 4.42 | 3.33 | 1.09 |
| LHMS-2 | 323.51 | 0.39 | 3.90 | 4.50 | 3.23 | 1.27 |
| LHMS-3 | 709.69 | 0.51 | 3.90 | 4.50 | 3.35 | 1.15 |
| LHMS-5 | 543.36 | 0.44 | 3.90 | 4.50 | 3.12 | 1.38 |
Notation: SBET = BET specific surface area; VP = total pore volume; d-spacing = Bragg spacing (= 2π/q*), where q* is the value of q at the maximum in the (100) peak for the p6mm mesostructure; a = unit cell parameter (= 2d100/√3 for p6mm structure); DKJS = mesopore diameter at the maximum in the PSD curve determined by KJS method; W = pore wall thickness (=a − DKJS).