Skip to main content
. 2018 Oct 22;8(63):35878–35887. doi: 10.1039/c8ra06989a

Fig. 7. (a) CV curves measured at different potential windows at a scan rate of 50 mV s−1, (b) GCD curves in different potential windows at the current density of 5 A g−1, (c) CV curves at different scan rates ranging from 10 to 500 mV s−1 within the potential window of 0–1.6 V, (d) galvanostatic charge/discharge curves at different current densities, and (e) cycling stability and coulombic efficiency at a constant current density of 5 A g−1 of the 1.5 at% Cu-doped Mn3O4//G ASC. (f) Ragone plots of the 1.5 at% Cu-doped Mn3O4//G ASC compared with other Mn3O4 based ASC.